摘要
We have investigated the role of the ambient gas nature and pressure in the structure and appearance of the laser treated zone. and the influence of the total duration and temporal shape of laser pulse with the laser tight being λ= 10.6μm wavelength incident upon a metallic surface at intermediate taser intensities of 107-108 W / cm2. A plasma is accompanied by the action of the laser pulse, It acts as an active moderator among laser beam and target thus determining the final status of the contact surface
We have investigated the role of the ambient gas nature and pressure in the structure and appearance of the laser treated zone. and the influence of the total duration and temporal shape of laser pulse with the laser tight being λ= 10.6μm wavelength incident upon a metallic surface at intermediate taser intensities of 107-108 W / cm2. A plasma is accompanied by the action of the laser pulse, It acts as an active moderator among laser beam and target thus determining the final status of the contact surface