摘要
The internal oxidation behavior of Pd-40Ag-1M(M=Zr,Y)alloy wires has been studied in air at 800—1200℃.The relationship between the internal oxidation depth ξ and the reaction time t can be expressed as ξ= Kt^n,where n=0.5—0.75.The higher the temperature,the larger the value of n is.The active elements Zr and Y show different internal oxidation characters.For the alloys eontaining Zr,the oxidation rate along the grain boundaries is about twice as high as that in grains,and“lateral oxidation”exists along the grain boundaries.For the alloys containing Y,the oxidation rates in grains and along the grain boundaries are roughly the same,and there is no“lateral oxidation”along the grain bounda- ries.The activation energies of both alloys are in the range of 120—150kJ/mol.Some prop- erties for oxidized alloys were studied.The mechanisms of the internal oxidation were dis- cussed.
The internal oxidation behavior of Pd-40Ag-1M(M=Zr,Y)alloy wires has been studied in air at 800—1200℃.The relationship between the internal oxidation depth ξ and the reaction time t can be expressed as ξ= Kt^n,where n=0.5—0.75.The higher the temperature,the larger the value of n is.The active elements Zr and Y show different internal oxidation characters.For the alloys eontaining Zr,the oxidation rate along the grain boundaries is about twice as high as that in grains,and“lateral oxidation”exists along the grain boundaries.For the alloys containing Y,the oxidation rates in grains and along the grain boundaries are roughly the same,and there is no“lateral oxidation”along the grain bounda- ries.The activation energies of both alloys are in the range of 120—150kJ/mol.Some prop- erties for oxidized alloys were studied.The mechanisms of the internal oxidation were dis- cussed.