摘要
介绍了某地高硫白钨矿石浮选药剂条件试验研究。在磨矿细度-200目占70%-75%的磨矿条件下,预先脱硫浮选,再常温浮选白钨,得到白钨精矿品位62.87%,回收率为84.33%。结果表明,此选矿工艺可有效处理该地区高硫白钨矿石。
Flotation reagent condition tests were conducted. Flotation tests were made on a high-sulfur scheelite. Under the condition of grinding fineness -200 mesh 70% -75%, a flotation desulfurization test was conducted in advance and then flotation of scheelite was carried out at atmospheric temperature. It achieved a scheelite concentrate with a grade of 62.87% and a recovery of 84.33%. The results indicated that this beneficiation process could deal with the high-sulfur scheelite in this area effectively.
出处
《现代矿业》
CAS
2009年第4期34-35,共2页
Modern Mining
关键词
白钨矿
常温浮选
预先脱硫浮选
Scheelite
Floatation at atmospheric temperature
Desulfurization floatation in advance