摘要 由于Mn,Cu,Pb,Zn,As等元素干扰与包裹,砷锰粘土型金银矿中金银的氰化浸出效果较差。矿物与催化溶液反应3~5h后,用炭浆法可以使金的浸出率从70%提高到91%~93%,银的浸出率从6%~10%提高到80%~90%,金银的氰化配合反应速度加快。试验对开发利用砷锰粘土金银矿资源具有很大的现实意义。 Because of the disturbance and coating of Mn, Cu, Pb, Zn, As etc. , the leaching effect of gold and silver from the arsenic manganese clay-type kustelite is no good. The gold and sliver leaching rate could be improved from 70% to 91%-93% and 6%-10% to 80%-90% respectively by the carbon pulp process after 3 -5 h reaction between clay-type kustelite with arsenic and manganese and the catalystsolutionand speed of the cyaniding coordination reaction was improved greatly.
出处 《稀有金属》 EI CAS CSCD 北大核心 2009年第2期272-275,共4页 Chinese Journal of Rare Metals
关键词 砷锰粘土金银矿 催化溶液 氰化 arsenic manganese clay-type kustelite catalyzed solution cyaniding gold silver
  • 相关文献

参考文献6

二级参考文献12

共引文献29

同被引文献27

引证文献3

二级引证文献33

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部