期刊文献+

微波加热法制备CaNiO_3光催化材料的研究 被引量:1

Preparation of Perovskite-type SrNiO_3 Photocatalyst Material by Microwave Heating Method
下载PDF
导出
摘要 提出一种新的制备CaN iO3光催化材料的方法,微波加热法.实验确定其最佳制备条件为:微波功率560W,微波加热时间30m in,煅烧温度700℃和煅烧时间5h;对在该条件下制备的催化剂进行了XRD表征.在可见光条件下,以模拟染料酸性大红废水为目标物,对催化材料的光催化性能进行了研究,结果表明微波加热法制备的光催化材料具有较高的光催化降解性能,染料降解率最高可达98%. A new microwave heating method for preparation of CaNiO3 photocatalyst material is described. The optimum preparation conditions are that the microwave power is 560W, the microwave heating time is 30min, the calcination temperature is 700℃ and the calcination time is 5h. The compound is measured by X-ray diffraction. In visible light and under the conditions of simulated fuel waste water, the photocatalytic properties of the catalyst material are studied. The results show that the photocatalytie material prepared by that microwave heating has a high photocatalytic performance of degradation, and the degeneration rate of the dye may reach 98%.
出处 《沈阳理工大学学报》 CAS 2009年第1期22-25,共4页 Journal of Shenyang Ligong University
关键词 钙钛矿复合氧化物 微波 光催化材料 CaNiO3 perovskite-type mixed oxide microwave photocatalyst material CaNiO3
  • 相关文献

参考文献8

二级参考文献91

共引文献239

同被引文献9

引证文献1

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部