3270m^3高炉水冷钢砖的铸造生产工艺

Casting Process of Water-cooling Adamantine Clinker of Blast Furnace
下载PDF
导出
摘要 通过对水冷钢砖的结构分析,找出铸造过程中的难点,采用设计合理内冷铁和仿真模拟验证,保证水管不被熔化并形成顺序凝固,采用脱落式芯盒和嵌入式定位,保证螺栓孔、固定栓尺寸位置,采用水玻璃七O砂与铬铁矿砂配合使用,解决螺栓孔难以铸出问题,设计使用专用定位工装,保证各部位尺寸准确,提高铸造质量。 Through the structural analysis of water cooling adamantine clinker, we can find out the difficulties in the casting. Adopting the rational-designed inner chill and analogue simulation verification can ensure that water pipe cann't be melt and make directional solidification. Adopting knockout core box and embedded positioning can ensure the size and position of the bolt holes and dead bolts. Adopting sodium silicate 70 sand and chromite sand together can help solve the problem of casting bolt holes. Adopting the well-designed special positioning jig can ensure the accuracy of the size of every part to improve the quality of casting.
作者 郭洪涛 郭林
出处 《铸造设备研究》 2009年第2期15-17,共3页 Research Studies On Foundry Equipment
关键词 水冷钢砖 内冷铁 仿真模拟 顺序凝固 嵌入式定位 water cooling adamantine clinker, inner chill, analogue simulation, directional solidification, embedded positioning
  • 相关文献

参考文献1

  • 1中国机械工程学会铸造分会.铸造手册第5卷铸造工艺(2版)[M].北京:机械工业出版社,2003.

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部