摘要
在高温形变后,把超低碳钢在700~920℃之间保温,以此作为开轧温度(FET),测定钢的晶粒度、应力-应变曲线,并进行显微组织观察。试验的结果是在铁素体已热轧、退火后可得高塑性。
After high temperature deformation,ultra low carbon steel is held between 700 ̄920℃,being as the temperature for the first pass.Crystal grain size,stressstrain curve of the steel are determined and microstructures are analyzed.The test results show that ferrite hot rolled and annealed has high plasticity.
出处
《鞍钢技术》
CAS
1998年第3期30-32,37,共4页
Angang Technology
关键词
轧制温度
超低碳钢
塑性
轧制
rolling temperature ultra low carbon steel plasticity