摘要
合成了AA/MA/AM/MM多元共聚物,并对所得产品进行了碳酸钙静态阻垢实验,探讨了共聚物的分子量、投加量、溶液的pH值、温度、恒温时间等因素与共聚物阻垢率的关系,并用扫描电子显微镜观测了碳酸钙晶形的变化,结果表明,AA/MA/AM/MM多元共聚物阻垢性能较好,该共聚物使碳酸钙晶形发生了畸变。
A series of acrylic acid/maleic anhydride/acrylamide/methylmethacrylate copolymers in sodium salt were prepared and tested as scale inhibitor in laboratory. The effect of AA/MA/AM/MM copolymer molecular mass, concentration,pH value, temperature and the time of constant temperature on the ratio of scale inhibition of copolymers were discussed. It was found that AA/MA/AM/MM copolymer had excellent properties of inhibiting CaCO3 scale and caused CaCO3 crystal distortion.
出处
《工业水处理》
CAS
CSCD
1998年第3期30-32,共3页
Industrial Water Treatment
关键词
多元共聚物
共聚物
阻垢剂
性能
acrylic acid/maleic anhydride/acrylamide/methylmethacrylate,scale inhibitor,ratio of scale inhibition