摘要
Microstructures of as-cast Al-Mg-Si-Mn alloys with and without Sc and Zr were investigated by optical microscopy, scanning electronic microscopy(SEM) and energy dispersion spectrum analysis. Addition of 0.2%-0.4% Sc can refine the grain size and change the growth morphology from dendritic to fine equi-axial crystal. The higher the addition of Sc, the finer the as-cast grain size. The tensile strength is increased by more than 30% with 0.4% Sc. Moreover, an addition of 0.1%-0.2% Zr is able to refine grain size and change the growth morphology from dendritic to equi-axial grain too, but less effective. However, Zr is found to increase the ductility of the cast alloys, and the elongation is increased to 11.97% with 0.2% Zr.
Microstructures of as-cast Al-Mg-Si-Mn alloys with and without Sc and Zr were investigated by optical microscopy, scanning electronic microscopy(SEM) and energy dispersion spectrum analysis. Addition of 0.2%-0.4% Sc can refine the grain size and change the growth morphology from dendritic to fine equi-axial crystal. The higher the addition of Sc, the finer the as-cast grain size. The tensile strength is increased by more than 30% with 0.4% Sc. Moreover, an addition of 0.1%-0.2% Zr is able to refine grain size and change the growth morphology from dendritic to equi-axial grain too, but less effective. However, Zr is found to increase the ductility of the cast alloys, and the elongation is increased to 11.97% with 0.2% Zr.
出处
《中国有色金属学会会刊:英文版》
CSCD
2009年第3期540-544,共5页
Transactions of Nonferrous Metals Society of China