摘要 In order to control welding stress and distortion, a new welding with trailing peening method based on the electromagnetic hammer was developed. This method uses the idea of constant frequency pulse width modulation for designing the control circuit of peening force and peening freqneney. The peening force can be adjusted between 0 and 1 000 N and the peening frequency ranges from 0 to 25 Hz. Peening force is applied to the weld metal and the weld toe during the welding by peening head. The experiments show that the method is portable and flexible, and it can adjust the distribution state of welding residual stress, making grain refinement. When the peening force is changed to 700 N and the peening frequency to 3 Hz, both the transverse and longitudinal residual stresses will drop obviously. In order to control welding stress and distortion, a new welding with trailing peening method based on the electromagnetic hammer was developed. This method uses the idea of constant frequency pulse width modulation for designing the control circuit of peening force and peening freqneney. The peening force can be adjusted between 0 and 1 000 N and the peening frequency ranges from 0 to 25 Hz. Peening force is applied to the weld metal and the weld toe during the welding by peening head. The experiments show that the method is portable and flexible, and it can adjust the distribution state of welding residual stress, making grain refinement. When the peening force is changed to 700 N and the peening frequency to 3 Hz, both the transverse and longitudinal residual stresses will drop obviously.
出处 《China Welding》 EI CAS 2009年第2期65-69,共5页 中国焊接(英文版)
基金 The work was supported by the Natural Science Foundation of Hebei Province of China under Grant No. E2006000528.
关键词 welding with trailing peening welding stress peening force peening frequency welding with trailing peening, welding stress, peening force, peening frequency
  • 相关文献

参考文献7

二级参考文献22

  • 1关桥,张崇显,郭德伦.动态控制的低应力无变形焊接新技术[J].焊接学报,1994,15(1):8-15. 被引量:46
  • 2刘伟平,田锡唐,张修智.一种防止高强铝合金焊接热裂纹产生的新方法[J].焊接学报,1995,16(2):106-111. 被引量:15
  • 3王引真,贺勇,王忠平,高大路,贺运佳.热应变对2090铝锂合金焊接热影响区显微组织和力学性能的影响[J].材料科学与工艺,1996,4(3):81-85. 被引量:6
  • 4杨愉平.反应变法防止高强铝合金薄板焊接热裂纹的研究[M].哈尔滨:哈尔滨工业大学,1995..
  • 5郭绍庆.高热裂敏感铝合金薄板焊接热裂与变形的控制研究[M].哈尔滨:哈尔滨工业大学,1999..
  • 6第一工业机械部哈尔滨焊接研究所.焊接裂缝金相分析图谱[M].哈尔滨:黑龙江科学技术出版社,1981..
  • 7[1]Koichi Masubuchi. Research activities examine residual stresses and distortion in welded structures. Welding Journal, 1991, (12):41~46
  • 8[2]Guan Q, Guo D L, Li C Q. Low stress non-distortion (LSND) welding-a new technique for thin material. Welding in the World, 1994, 33(3):160~167
  • 9周万盛.航天贮箱材料及其焊接性[J].宇航材料工艺,1986,(5):57-59.
  • 10徐文立.随焊锤击控制铝合金薄板焊接应力变形及接头质量的研究[M].哈尔滨:哈尔滨工业大学,2001..

共引文献58

同被引文献5

引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部