摘要
柳钢高炉采用精料和小高压操作,同时加强了操作管理,使高炉利用系数在较短的时间里提高0.504t/(m3·d),焦比降低96kg/t。
The BF at Liuzhou Iron and Steel(Group) Company is operated with benefi ciated burden materials,adopting little over pressure at top and improved management The utilization coefficient has been increased by 0 504 t/(m 3·d)and the coke ratio has been decreased by 96 kg/t in a short period
出处
《钢铁》
CAS
CSCD
北大核心
1998年第8期9-12,共4页
Iron and Steel
关键词
强化冶炼
利用系数
焦比
高炉
炼铁