研究以0.88dtex细特腈纶丝束为主要原料在Seydel-679型拉断机上生产细特腈纶正规条,并与3.33dtex腈纶收缩条混纺,开发生产仿羊绒腈纶条。结果表明,生产仿羊绒腈纶纤维条的适宜工艺为:拉断工序拉伸倍数6.05—6.27,再割区隔距比常规工艺大5mm,卷曲箱压力略大,汽蒸压力为0.15~0.3MPa;针梳工序正规条与收缩条配比为52:48,降低针板号数,退卷曲区牵伸倍数1.15~1.3,梳箱喂入区牵伸倍数0.98,主牵伸倍数6—8,前罗拉隔距45mm。
0.88dtex acryhc tow was used as main raw material and processed on Seydel -679 stretch breaking machine and blended with 3.33dtex shrinking acryhc top to develop cashmere - hke acrylic top. The result shows that cashmere - hke acrylic top can be produced based on the following parameters : total stretch ratio in stretch breaking is 6.05 - 6.27, recutting gauge is 5mm bigger than normal process. Steam pressure is 0.15 - 0.3Mpa, proportion of regular top and shrinking top is 52:48 ,cutting down needle plate number,draft multiple in uncrimping zone is 1.15 - 1.3,draft multiple in comb box feeding zone is 0.98,main draft multiple is 6 - 8 and front roller gauge is 45mm.
出处
《上海纺织科技》
北大核心
2009年第10期39-41,45,共4页
Shanghai Textile Science & Technology
关键词
腈纶
纺羊绒条
纤维条
产品开发
acrylic
Cashmere - like top
top
product developing