摘要
河北某萤石矿因原矿品位低、萤石与石英嵌布粒度极细、有一定程度的风化而难选,原选矿生产只能获得CaF2品位在88%左右的精矿,影响销售。为此,对该矿石重新进行了选矿工艺试验研究。试验针对矿石特点,采用一次精选精矿再磨、7次精选的浮选流程,可获得CaF2品位为97.23%,S iO2含量为2.36%,CaF2回收率为70.56%的萤石精矿,提高了精矿质量,为企业扩大产品市场空间提供了技术支持。
Due to low grade raw ores, fine-grained dissemination of fluorite and quartz, and some weathering issues, the fluorite in Hebei province belongs to the refractory one. CaF2 concentrate only grading at about 88% by the former beneficiation can not reach a good sale. Therefore, the beneficiation experiments are carried out again for this ore. In view of the ore characters, a flotation flow sheet consisting of one-stage cleaning flotation regrinding and seven stage cleaning flotation was selected. Finally,fluorite concentrates with CaF2of 97.23% ,and SiO2 of 2.36% ,and CaF2 recovery of 70.56% were obtained,and the quality of production was improved greatly, providing the technical support to get a large market for the mine enterprise.
出处
《金属矿山》
CAS
北大核心
2009年第10期104-107,共4页
Metal Mine
关键词
低品位难选萤石矿
再磨
浮选
精矿品位
Low grade refractory fluorite, Regrinding, Flotation, Concentrate grade