摘要
分析了新疆某钼矿的矿石性质,进行了粗选条件试验,对比研究了一段磨矿、一段再磨和二段再磨工艺。结果表明,通过二段再磨、8次精选,钼精矿品位为44.31%,回收率81.96%。
The ore property of a Molybdenum Mine in Xinjiang was analyzed, and then the condition tests for rough separation were carried out. The comparison of 1-stage grinding with 2-stage grinding showed that a Molybdenum concentrate grading 44.31% at an 81.96% recovery can be achieve after 2-stage regrinding and 8 times cleaning separation.