摘要
以硫酸亚铁为原料,氯气为氧化剂,氢氧化钙和稳定剂为中和剂,当溶液pH值为1.90~2.00,氧化时间为0.5h,铁离子质量浓度为0.08mol/L时,可以合成盐基度为56%的聚合氯化硫酸铁,液收为75%
Using ferrous sulfate as raw material, chlorine as oxidant, calcium hydroxide and stabilizer as neutralizer, when solution pH value is 1.90~2.00, oxidation time is 0.5 h and mass concentration of ferric ion is 0.08mol/L, can synthesize ferric sulfate polychloride with salinity of 56% and solution yield rate is 75%.
出处
《黑龙江石油化工》
1998年第3期18-20,共3页
Heilongjiang Petrochemical Technology
关键词
聚合氯化硫酸铁
盐基度
絮凝剂
合成
ferric sulfate polychloride oxidant neutralizer salinity