摘要
为满足工程对蒸压加气混凝土砌块(AAC)墙体裂缝控制质量要求,通过多项类似工程墙体裂缝调查统计资料,分析墙体裂缝的破坏形态和产生原因,根据主要裂缝性状从人员、机具、材料、方法以及环境方面分析主要影响因素,并采取相对应施工技术解决对策,达到了预期目的。
To meet the quality requirement of crack controlling for Autoclaved Aerated Concrete(AAC) blocks wall,the damage forms and its causing for cracks were analyzed by means of research statistic on crack of wall in similar projects.According to major cracking character,major influencing factors were analyzed from the points such as person,implement,material,method and environment.By adopting corresponding construction technologies to solve the problems,expected target was achieved finally.
出处
《山西建筑》
2009年第36期134-135,共2页
Shanxi Architecture