摘要
通过实验,得到了优良、低价和无毒的精炼渣复合发泡剂配方:CaCO370%~80%,MgCO36%~10%,Na2CO35%~10%,NaCl2%~6%,SiC8%~12%。
Based on the experiment, the excellent, cheap and non-toxic compound foaming ingredient (% ): CaCO370~ 80, MgCO36 ~ 10, Na2CO3 5 ~ 10, NaCI 2~ 6, SiC 8 ~ 12 for refining slag was obtained.
出处
《特殊钢》
北大核心
1998年第6期24-26,共3页
Special Steel