摘要
安钢两座2000m3级高炉铁口近期相继出现烧坏铁口框架,铁口区域炉壳损坏,危及铁口区冷却壁,影响铁口安全和高炉长寿生产。通过分析原因,妥善处理,制定实施预防铁口损坏的措施,效果较好。
The iron notch of the two 2000 m^3 BF in ANYANG steel were damaged one after the other in recent, which caused furnace shell burning_out in tap hole area, not only imperiling the cooling wall in tap hole area, but also harming the salty and life on iron notch. According to cause analysis and proper treatment, the measures were worked out to protect the frame of iron hole from being damaged.
出处
《河南冶金》
2010年第1期44-46,共3页
Henan Metallurgy
关键词
高炉
铁口
处理预防措施
blast furnace iron notch prevention