摘要
原矿为高含泥高氧化率低品位铜矿。根据矿石的工艺矿物学特性,开展"直接浮选"、"预先脱泥+浮选"和"酸浸"三种工艺流程试验。试验结果表明,"酸浸"是最佳的提铜工艺流程。在较佳的酸浸工艺条件下,可获得铜浸出率92.09%,硫酸耗量54kg/T的技术经济指标。
The raw ore is the high mud, high oxidation and low grade Cu ore. According to the technological and mineralogical characteristics of it, we have carried out "direct floatation", "pre - remove of mud + floata- tion" and "acid immersion" 3 technological flow charts, which shows that the "acid immersion" is the best one. Under the good "acid immersion" technological condition, the Cu leachability can be 92. 09% and the con- sumption of sulfuric acid 54 kg/t.
出处
《云南地质》
2010年第1期105-108,共4页
Yunnan Geology
关键词
氧化铜矿
高含泥
低品位
酸浸
浮选
云南兰坪
Cu Oxide Ore
High Mud
Low Grade
Acid Immersion
Floatation
Lanping, Yunnan