通过对陶瓷厂污水站水池裂缝成因的分析,提出了控制裂缝的主要措施,并通过实例加以印证。
In this paper,the formation causes of crevices in sevage centre structures of ceramic factory were analyzed,and main measures for controlling the creviceswere put forward and were confirmed by examples.