摘要
采用工业级DCPD,研究了油酸改性DCPD不饱和聚酯树脂的合成工艺及制漆性能。试验结果表明:在树脂合成过程中加入5%~9%油酸,合成的树脂具有优良的气干性,而且柔韧性和防绿化性大为提高,满足涂料用不饱和树脂的要求。
With industrial grade DCPD, the synthesis process and paint performance of oleic acid modified DCPD unsaturated polyester resin were studied, experimental results showed that the synthetic resin not only had good air drying, but also greatly improved the flexibility and greening resistance by means of addition of 5%-9% oleic acid so as to meet the requirement of unsaturated resins for the coatings.
出处
《上海涂料》
CAS
2010年第4期45-46,50,共3页
Shanghai Coatings
关键词
油酸
DCPD
改性不饱和聚酯树脂
家具涂料
oleic acid
DCPD
modified unsaturated polyester resin
furniture coatings