摘要
以平顶山庚组高硫煤粉为煤样,利用实验室自制的永磁强磁选机进行分选试验,发现:随着颗粒粒径的增大,其灰分、硫分也随之增加;该磁选机的最佳分选粒度范围为0.25~0.5mm;磁选脱除的主要是煤中黄铁矿硫,而硫酸盐硫和其他有机硫则变化不大。
With the high-sulfur coal powder from Pingdingshan 7th Coal Seam as the coal sample, using laboratorymade high intensity magnetic separator for sorting, found that: As the particle size increases, the ash, sulfur also increases; the optimum sorting size range is from 0.25 mm to O. 5mm; magnetic removal is mainly pyrite sulfur in coal, while the sulfate sulfur and other organic sulfur change little.
出处
《洁净煤技术》
CAS
2010年第1期32-34,20,共4页
Clean Coal Technology
关键词
煤粉
磁选
脱硫率
黄铁矿硫
pulverized coal
magnetic separation
desulfurization rate
pyrite sulfur