弹簧钢100t DC EAF-LF-VD流程无铝脱氧工艺实践 被引量:2

Process Practice of Non-Aluminum Deoxidation for Spring Steel Steelmaking Production by 100 t DC EAF-LF -VD Flow Sheet
下载PDF
导出
摘要 EAF-LF-VD冶炼60Si2MnA和55CrSiA弹簧钢时EAF出钢过程加17~23 kg/t低铝硅铁(Al含量≤0.50%)脱氧,LF补加3~6 kg/t硅铁,并控制精炼渣的碱度≤2.5,可控制[Als]≤60×10^(-6),总[O](9~20)×10^(-6),A类夹杂级别≤0.5,B类≤0.5,C类≤1.5,D类≤0.5。用该脱氧工艺冶炼的钢水可浇注性强,适合大批量工业性生产。 In spring steel 60Si2MnA and 55CrSiA steelmaking by EAF-LF-VD, it is available to control [ Als] ≤ 60 ×10^-6, the total [ O] (9 - 20) ×10^-6, and get the rating of A series inclusion ≤0. 5, B series ≤0. 5, C series ≤ 1.5 and D series ≤0. 5 by adding 17 - 23 kg/t low aluminum ferrosilicon (Al content ≤0. 50% ) during EAF tapping, adding more 3 - 6 kg/t ferrosilicon during LF refining and controlling basicity of refining slag ≤2. 5. The molten steel produced by this deoxidation process has excellent castability being available for mass production.
出处 《特殊钢》 北大核心 2010年第3期38-40,共3页 Special Steel
关键词 60Si2MnA、55CrSiA弹簧钢 无铝脱氧 工艺实践 Spring Steel 60Si2MnA, 55CrSiA, Non-Aluminum Deoxidation, Process Practice
  • 相关文献

同被引文献13

引证文献2

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部