摘要
分析了大中型呋喃树脂砂铸钢件粘砂缺陷的形成原因,介绍了为防止粘砂缺陷形成,在树脂砂原材料的选择、型砂制备工艺参数控制、造型操作、涂料涂刷、浇注温度等方面应采取的措施以及要重视的问题。
The reasons causing burning-on and metal penetration defect of medium-large furan resin sand steel castings wereanalyzed. An introduction was made to the measures to be taken and problems to be noticed in order to prevent burning-onand metal penetration defects in the aspects of raw materials choice of furan resin sand, control of molding sand preparingprocess parameters, molding operation, coating brushing, pouring temperature and so on.
出处
《现代铸铁》
CAS
2010年第2期58-60,共3页
Modern Cast Iron
关键词
呋喃树脂砂
铸钢件
粘砂
furan resin sand
steel casting
burning-on and metal penetration