Sc_2(WO_4)_3的高温快速合成及特性研究 被引量:2

Synthesis and Properties of Sc_2(WO_4)_3 by High-heat and Fast Way
下载PDF
导出
摘要 首次采用高温快速合成方法成功地将比例适当的Sc2O3和WO3粉末合成了形貌良好的Sc2(WO4)3材料,并利用多种分析手段对该材料进行分析.拉曼光谱分析说明在合适工艺参数下高温快速烧结可避免原料挥发,使原料完全参与反应.X射线衍射(XRD)分析表明合成物主要是Sc2(WO4)3材料,属空间群Pnca,具有正交结构,可以呈现负热膨胀特性.扫描电镜(SEM)发现合成物晶粒分散性好,呈链状并互相纠缠在一起.能量散射光谱(EDS)分析显示合成物内部成分分布均匀. Sc2(WO4)3 ceramic had been successfully and rapidly synthesized with a proper proportion of Sc2O3 and WO3 by high - heat and fast way for the first time. The microstructure observation, component and phases analysis of this ceramic were performed by a Raman spectrometer, scanning electron microscopy, energy -disoersive soectrometer and X- ray diffractometer.
出处 《通化师范学院学报》 2010年第4期29-31,共3页 Journal of Tonghua Normal University
关键词 高温快速合成 负热膨胀 拉曼光谱 X射线衍射 Sc2(WO4)3 high -heat and fast synthesis negative thermal expansion Raman spectrum X -ray diffraction Sc2(WO4)3
  • 相关文献

参考文献4

  • 1I. D. Brown and D. Altermatt, Bond - Valence Parameters Obtained from a Systematic Analysis of the Inorganic Crystal Structure Database [ J ]. Acta Crystallographica Section B, 1985,41:244 - 247.
  • 2Rougier A, Portemer F, Quede A. Charactezation of pulsed laser deposited WOs thin films for electrochromic devices[ J ]. Surface Science, 1999, 153(1) :1 -9.
  • 3Nandini Garg, Chitra Murli, A. K. Tyagi, Surinder M. Sharma. Phase transitions in Sc2 ( WO4 ) 3 under high pressure [ J ]. Physical Review,2005, 72,064106:1 -6.
  • 4M. Maczka, K. Hermanowicz, J. Hanuza. Phase transition and vibrational properties of A2 ( BO4 ) 3 compounds ( A = Sc, In; B = Mo, W) [ J ]. Molecular Structure, 2005,744 - 777 : 283 - 288.

同被引文献26

引证文献2

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部