裂纹扩展片技术在弧形面上半椭圆表面裂纹长度测试中的应用

Application of Krak-gage Technology on Measuring Half-ellipse Surface Crack Length on Arc
下载PDF
导出
摘要 简述了裂纹扩展片技术的研究现状和测试原理,标定出应用在单臂悬梁试样弧形面上的单片和串联双片10mm裂纹扩展片的裂纹长度增量与电压增量关系方程。通过扩展片与试样裂纹扩展同步性研究,证明了裂纹扩展片技术应用于弧形面上半椭圆表面裂纹长度测试的可行性。 Current research status and testing principle of krak gage technology was described.Based on the technology,half-ellipse surface crack length on arc of single-cantilever beam bonded specimen was successfully measured,the equation about crack length and voltage of 10 mm single and double krak-gage had been achieved. Which showed it was capable that krak-gage technology was applicated in measuring half-ellipse surface crack length on arc.
出处 《理化检验(物理分册)》 CAS 2010年第5期303-305,312,共4页 Physical Testing and Chemical Analysis(Part A:Physical Testing)
关键词 裂纹扩展片 弧形面 半椭圆表面裂纹 裂纹长度 krak-gage arc half-ellipse surface crack crack length
  • 相关文献

参考文献9

  • 1崔玉华,邢志强.疲劳裂纹测试的裂纹扩展片技术[J].理化检验(物理分册),1994,30(5):44-45. 被引量:1
  • 2PARIS P C, HAYDEN B R. A new system for fatigue crack growth measurement and control [C]// ASTM Symposium on Fatigue Crack Growth. Pittsburgh, PA:[s. n. ],1979.
  • 3PETER K L, HELM E J, ENGING. Corrosion fatigue crack propagation testing with KRAK-GAGE in salt water[J]. Fract Mech, 1983,18: 121-131.
  • 4HARTMANN H R , CHURCHILL R W. Krakgage, a new transducer for crack growth measurements[C]// SESA Fall Meeting. Keystone, CO: [s.n. ], 1981.
  • 5PETER K L, WILLIAM A L, LEWIS D R, et al. Krak-gages for automated fatigue crack growth rate testing[C]// Automated Test Methods for Fracture and Fatigue Crack Growth(STP877). [s. l. ]: [s. n, ], 1985:177-196.
  • 6PHOPLONKER M A, BYRNE J, DUGGAN T V, et al. Near-threshold fatigue crack growth in aluminum bronze alloy[J]. ImeehE, 1986,C227:137-144.
  • 7MCRAE K I. Application of "Fractomat/Krak-gage" to Crack Growth Measurement in Structural Component[M]. Victoria, B. C, Canada:Defenee Research Establishment Pacific, Research and Development Branch, 1982.
  • 8PRABHAKARAN, RAMAMURTHY. Method of Continuously Determining Crack Length: U. S. , 5, 227,731[P]. 1993-07-13.
  • 9NICHOLLS, JOHN Rayment. Measuring Device: U. S. ,6,172,511[P]. 2001-01-09.

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部