摘要 对张天渠油田注水系统的注入水进行了离子分析,在采用化学分析、XRD、SEM等手段分析了典型结垢部位垢样的基础上,运用饱和指数法及Scalechem分析软件对油田注水系统在不同压力条件下的结垢类型及趋势进行了预测,并提出了综合防垢措施。 This paper carried on the ion analysis for the injected water from the water injection system of Zhangtianqu Oilfield. On the basis of analyzing the typical parts of scaling sample by using chemical analysis, XRD and SEM , the saturation index method and SCALECHEM analytical software system were used to predict the types and trends of scaling under different water stress conditions. Finally the paper puts forward comprehensive anti-scaling measures.
出处 《安全与环境工程》 CAS 2010年第4期118-122,共5页 Safety and Environmental Engineering
关键词 油田 注水系统 结垢 腐蚀 防垢措施 oilfield water injection system scaling corrosion anti-scaling measure
  • 相关文献

参考文献5

  • 1祝海涛,李毓枫,史瑞雪,张丽平.油田层产出水结垢原因与防治对策研究[J].石油化工应用,2008,27(2):55-60. 被引量:19
  • 2SY/T5523-2000,油气田水分析方法[S].
  • 3SY/T5329-94.碎屑岩油藏注水水质推荐指标及分析方法[S].[S].,..
  • 4SY/T0026-1999,水腐蚀测试方法[S].
  • 5李章亚.油气田腐蚀与防护技术手册[M].北京:石油工业出版社,1996.

二级参考文献2

共引文献66

同被引文献40

  • 1郭润生,孙红江,刘杰.韩渠油田注水管线的结垢腐蚀与防治[J].海洋石油,2001,21(3):49-51. 被引量:4
  • 2李闽,李士伦,杜志敏.沥青沉积与地层伤害[J].新疆石油地质,2003,24(5):479-481. 被引量:9
  • 3党娟华,罗跃.油田污水阻垢剂研究进展[J].涂料涂装与电镀,2005,3(3):27-30. 被引量:10
  • 4王庆.东辛油田注水系统腐蚀结垢机理研究[J].石油化工腐蚀与防护,2007,24(1):25-28. 被引量:9
  • 5中华人民共和国国家发展和改革委员会.SY/TS523-2006油田水分析方法[s].北京:中国标准出版社,2006.
  • 6Salman M, A1-Hashem A, Carew J, et al. Control of scaling tendencies in an e{fluent water injection plant in west kuwait oil fields: Laboratory study[-J. SPE 81573,2003.
  • 7Kuang F, Wang J, Yan L, et al. Effects of sulfate-reducing bacte ria on the corrosion behavior of carbon steel[J]. Electrochimica Acta, 2007,52(20) 6084-6088.
  • 8Luna A S,da Costa A C A,Goncalves M M M,et aL The effects of surfactants on the estimation of bacterial density in petroleum samples[ J ]. Applied Biochemistry and Biotechnology , 2008, 147(42) 77-84.
  • 9Hubert C, Nemati M, Jenneman G, et al. Corrosion risk associat- ed with microbial souring control using nitrate or nitrite[J]. Ap- plied Microbiol Biotechnology, 2005,68 (2) z 272-282.
  • 10Herrera L K,Videla H A. Role of iron-reducing bacteria in cor- rosion and protection of carbon steel[J]. International Biodete- flotation and Biodegradation, 2009,63 ( 7 ) 891-895.

引证文献3

二级引证文献12

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部