期刊文献+

擦拭用复合纤维丝束生产工艺的研究

Production Process of Bicompoment Composite Fibers Tow for Wiping
下载PDF
导出
摘要 按照擦拭用复合纤维丝束本身特殊的质量要求和生产工艺制备低熔点热黏合皮芯复合纤维。就其生产工艺及设备、质量要求、工艺原理以及工艺参数进行探讨。主要工艺参数:PET特性黏度1.0dL/g,复合比(PE/PET)40/60,拉伸倍数3.5,拉伸温度85℃,卷曲温度90℃,松弛定形温度100~105℃,定形时间20min。产品质量可靠,能满足客户对纤维产品高强高模、优良卷曲回复率和高卷曲峰谷高度(一定的波峰角)的要求,并已获国家专利。 Bicomponent composite fibers tow for wiping,as a new application of low melt-point thermobonding,core sheath composite fibers,has its own special quality requirement and production process.The article presents the discussion on the production process,equipment,quality,process principle and parameter,i.e.,PET intrinsic viscosity 1.0 dL/g,composite ratio(PE/PET)40/60,drawing ratio 3.5,drawing temperature 85 ℃,crimping temperature 90 ℃,relax heat-setting temperature 100~105 ℃ for 20 min.The product quality is reliable and meets the customer requirement of high tenacity and modulus,perfect crimp recovery and higher crimp amplitude with certain peak angle.
作者 单正进
出处 《合成纤维》 CAS 2010年第8期35-37,共3页 Synthetic Fiber in China
关键词 增黏聚酯 复合比 卷曲回复率 卷曲波峰谷高度 viscosity increasing polyester composite ratio crimp recovery crimp amplitude
  • 相关文献

参考文献1

  • 1盐城市中联复合纤维有限公司,单正进.擦试用复合纤维丝束实用新型:ZL2007.2.0037650.9[P].2007.5.14.

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部