摘要 采用水热法合成了一系列不同化学计量配比的LaxSr1-xMnO3阴极粉体,并用XRD、SEM和电化学工作站分析设备等对粉体的晶体结构和微观形貌进行分析和表征。结果表明,当矿化剂KOH浓度为4-6mol/L,反应时间为50小时,温度为260-270℃时,能获得粒度均一具有典型钙钛矿结构的LaxSr1-xMnO3阴极粉体。 A series of LaxSr1-xMnO3 cathode powders were synthesized from materials mixed to different stoichiometric ratios by a hydrothermal method in this work.The crystal structure and microstructure of the powders were characterized by XRD,SEM and electrochemical analysis equipment.The results showed that LaxSr1-xMnO3 cathode powder of uniform size and typical perovskite structure can be obtained at the mineralizer KOH concentration of 4-6mol/L,reaction time of 50 hours and the temperature from 260-270 ℃.
出处 《陶瓷学报》 CAS 北大核心 2010年第3期387-390,共4页 Journal of Ceramics
基金 国际科技合作项目(编号:2009DFA51210) 国家自然科学基金(编号:50862004)
关键词 水热法 阴极 LaxSr1-xMnO3 矿化剂 电化学工作站 hydrothermal method cathode LaxSr1-xMnO3 mineralizer electrochemical workstation
  • 相关文献

参考文献7

二级参考文献24

共引文献34

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部