Ni-Cr微米复合镀层抗高温氧化性能研究 被引量:2

High Temperature Oxidation Behavior of Electrodeposited Ni-Cr Microcomposite Coatings
原文传递
导出
摘要 采用复合电沉积法制备出Cr颗粒含量不同的Ni-Cr微米复合镀层,该镀层由电镀Ni和微米Cr颗粒(~2.4μm)组成.900℃20 h高温氧化实验结果表明,当Cr含量接近32 mass%时,该复合镀层能够形成一层连续的Cr_2O_3氧化膜.通过对微米Cr颗粒含量不同的Ni-Cr复合镀层氧化性能的对比,讨论了其氧化机理. Ni-Cr microcomposite coatings were prepared on Ni-plates by co-electrodeposition of Ni with microparticles of Cr.The oxidation of the composite coatings at 900℃in air was investigated and then the formed oxide scales were examined by SEM with XRD.The results showed that continuous Cr_2O_3 scale could form on the composite coating when the Cr content was closely to 32 mass%.The oxidation behavior of the composite coatings was discussed in detail.
作者 李里 王福会
出处 《腐蚀科学与防护技术》 CAS CSCD 北大核心 2010年第5期367-370,共4页 Corrosion Science and Protection Technology
关键词 电沉积 Ni-Cr微米复合镀层 氧化 electrodeposition Ni-Cr microcomposite oxidation
  • 相关文献

参考文献10

  • 1Gggins C S, Pettit F S. Oxidation of Ni-Cr-Al alloys between 1000 ℃ and 1200℃ [J]. J. Electrochem. Soc., 1971, 118: 1782.
  • 2Nicholls J R, Hancock P, Al-Yasiri L H. Optimising oxidation resistance of MCrAl coating systems using vapour phase alloy design[J]. Mater. Sci. Tech., 1989, 5: 799.
  • 3Kofstad P. High temperature corrosion[M]. London and New York: Elsevier Applied Science, 1988: 132.
  • 4Koo C H, Yu T H. Pack cementation coatings on Ti3Al-Nb alloys to modify the high-temperature oxidation properties [J]. Surf. Coat. Technol., 2000, 126: 171.
  • 5Wang F, Tian X, Li Q, et al. Oxidation and hot corrosion behavior of sputtered nanocrystalline coating of superalloy K52[J]. Thin solid films, 2008, 516: 5740.
  • 6Bazzard R, Boden P J. Nickel-chromium alloy by codeposition: Part I-Codeposition of chromium particles in a nickel matrix[J]. Trans. Inst. Met. Finish., 1972, 50: 63.
  • 7张艳,张春林,彭晓,王福会.Cr颗粒尺寸对Ni-Cr复合镀层氧化行为的影响[J].中国腐蚀与防护学报,2006,26(2):85-88. 被引量:12
  • 8Zhang Y, Peng X, Wang F H. Development and oxidation at 800 ℃ of a novel electrodeposited Ni-Cr nanocomposite film[J]. Mater. Lett., 2004, 58: 1134.
  • 9Calvarin C, Molins R, Huntz A M. Oxidation mechanism of Ni-20Cr foils and its relation to the oxide-scale microstructure[J]. Oxid. Met., 2000, 53: 25.
  • 10Peng X, Li L, Wang F H. Application of AFM in a study of the selective oxidation behavior of materials during the early oxidation stage[J]. Scr. Mater., in press.

二级参考文献9

  • 1Atkinson H V.A review of the role of short-circuit diffusion in the oxidation of nickel,chromium and nickel-chromium alloys[J].Oxid.Met.,1985,24:177-197
  • 2Goward G W.Overview protective coatings-purpose role and design[J].Mater.Sci.Technol.,1986,2:194-199
  • 3Peng X,Ping D,Li T,et al.Oxidation behaviour of a Ni-La2O3codeposited film on nickel[J].J.Electrochem.Soc.,1998,145:389-398
  • 4Goward G W,Boone D H.Mechansims of formation of diffusion aluminide coatings on nickel-base superalloys[J].Oxid.Met.,1971,3:475-481
  • 5Nicholls J R,Hancocl P,Al-Yasiri L H.Optimising oxidation resistance of MCrAl coating systems using vapour phase alloy design[J].Mater.Sci.Technol.,1989,5:799-808
  • 6Wang F,Lou H.Oxidation behaviour and scale morphology of normai-grained CoCrAl alloy and its sputtered microcrystalline coating[J].Mater.Sci.Eng.,1990,A129:279-285
  • 7Lou H,Zhu S,Wang F,et al.Rehealing ability of oxide scale formed on microcrystalline K38G coating[J].Oxid.Met.,1995,43:317-329
  • 8Zhang Y,Peng X,Wang F.Development and oxidation at 800℃ of a novel electrodeposited Ni-Cr nanocomposite film[J].Mater.Lett.,2004,58:1134-1138
  • 9Zhou Y,Peng X,Wang F.Oxidation of a novel electrodeposited Ni -Al nanocomposite film at 1050℃[J].Scr.Mater.,2004,50:1429-1423

共引文献11

同被引文献93

引证文献2

二级引证文献9

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部