摘要 对碲铜复杂原料中碲贵金属采用了加压浸出工艺处理,研究了游离NaOH浓度、固液比、浸出时间、浸出压力、浸出温度对浸出效果的影响。研究结果表明,游离NaOH浓度为40g.L-1、固液比为1∶7、浸出时间为6h、浸出压力为0.9MPa、浸出温度为120℃时,碲浸出效果最好。贵金属碲以TeO2形态回收,试验结果碲回收率≥95%。 In this article,we apply autoclave leaching process of treatment for tellurium in complicated materials,and make some studies on the influences which concentration of NaoH,the ratio of solid to liquid,leaching time,leaching pressure and leaching temperature to the effect of leaching.The result shows that the leaching effect is the best with the conditions of Tellurium NaoH concentration of 40g·L-1,the solid to liquid rate of 1:7,leaching time of 6h,leaching pressure of 0.9MPa,leaching temperature of 120℃.If tellurium of precious metals is reclaimed in the shape of TeO2,the recovery rate will be over 95%.
作者 祝志兵
出处 《铜业工程》 CAS 2010年第3期49-51,共3页 Copper Engineering
关键词 浸出 加压 Tellurium leaching autoclave
  • 相关文献

参考文献2

二级参考文献2

  • 1王学文,吴义千,周(牛牛牛).分段中和逆流净化在铜阳极泥湿法冶金中的应用[Z].第三届国际湿法冶金会议.昆明:1998.
  • 2胡少华.净化渣中铜碲的回收[J].有色冶炼,1999,28(1):22-23. 被引量:5

共引文献36

同被引文献56

引证文献4

二级引证文献15

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部