期刊文献+

Preparation of Anhydrate Phosphogypsum Binders

Preparation of Anhydrate Phosphogypsum Binders
原文传递
导出
摘要 In this work,phosphogypsum(PG) with a small amount of lime was thermally pretreated at 450 ℃ to produce anhydrate gypsum for the purpose of searching new ways for utilization of waste PG. Additives,K2SO4 and one selected seed crystal(SC),were used as activator for anhydrate PG. The hydration characteristics of the anhydrate PG binders were investigated by determination of the setting time,the ratio of hydrated anhydrate PG,the compressive strength development,and the microstructure of the hardenite. The resistance to water was studied by measuring mass loss of binders exposed to hydrodynamic water. Results suggest that activated by K2SO4 and SC,anhydrate PG hydrates much more rapidly than that without additives. The anhydrate PG binder with K2SO4 and SC has proper setting time and good strength developments. SEM photos show that the set binders have hydrated products of rodlike and regularly shaped crystals. Those crystals connected closely,and the hardenite has a compact structure,which is beneficial to the obtainment of good properties. In this work,phosphogypsum(PG) with a small amount of lime was thermally pretreated at 450 ℃ to produce anhydrate gypsum for the purpose of searching new ways for utilization of waste PG. Additives,K2SO4 and one selected seed crystal(SC),were used as activator for anhydrate PG. The hydration characteristics of the anhydrate PG binders were investigated by determination of the setting time,the ratio of hydrated anhydrate PG,the compressive strength development,and the microstructure of the hardenite. The resistance to water was studied by measuring mass loss of binders exposed to hydrodynamic water. Results suggest that activated by K2SO4 and SC,anhydrate PG hydrates much more rapidly than that without additives. The anhydrate PG binder with K2SO4 and SC has proper setting time and good strength developments. SEM photos show that the set binders have hydrated products of rodlike and regularly shaped crystals. Those crystals connected closely,and the hardenite has a compact structure,which is beneficial to the obtainment of good properties.
出处 《武汉理工大学学报》 CAS CSCD 北大核心 2010年第17期193-195,200,共4页 Journal of Wuhan University of Technology
基金 support provided by the National Natural Science Foundation of China (Project NO.50802019) the Introduction of Research Personnel Foundation of Guizhou University(Project No.2008019)
关键词 anhydrate PG binders ACTIVATOR HYDRATION anhydrate PG binders activator hydration
  • 相关文献

参考文献11

  • 1Nurhayat Degirmenci. The Using of Waste Phosphogypsum and Natural Gypsum in Adobe Stabilization[J ]. Construction and Building Materials,2008(22 ) : 1220-1224.
  • 2Yang Mn, Qian J S, Pang Y. Activation of Fly Ash-lime Systems Using Calcined Phosphogypsum[J]. Construction and Building Materials,2008(5) : 1004-1008.
  • 3Taher M A. Influence of Thermally Treated Phosphogypsum on the Properties of Portland Slag Cement. Resources[J ]. Conservation and Recycling,2007(52/1) : 28-38.
  • 4Samia Azabou, Tahar Mechichi, Bharat K C, et al. Isolation and Characterization of a Mesophilie Heavy-metals-tolerant Sulfate-reducing Bacterium Desulfomierobium Sp [J ]. From an Enrichment Culture Using Phosphogypsum as a Sulfate Source. Journal of Hazardous Materials, 2007,140 (1-2) : 264-270.
  • 5Semra Coruh, Osman Nuri Ergun. Use of Fly Ash, Phosphogypsum and Red Mud as a Liner Material for the Disposal of Hazardous Zinc Leach Residue Waste[J]. Journal of Hazardous Materials,2010,173(1-3):468-473.
  • 6Mun K J, Hyoung W K, Lee C W, et al. Basic Properties of Non-sintering Oement Using Phosphogypsum and Waste Lime as Activator[J]. Construction and Building Materials, 2007, 21(6) : 1342-1350.
  • 7Guan B H, Yang L C, Wu Z B, et al. Preparation of a-calcium Sulfate Hemihydrate From FGD Gypsum in K, Mg-containing Concentrated CaCl2 Solution Under Mild Conditions[J]. Fuel,2009,88(7):1286-1293.
  • 8Xiao L G, Hui S S. Thermal Treatment and Utilization of Flue Gas Desulphurization Gypsum As an Admixture in Cement and Concrete[J]. Construction and Building Materials,2008,22(7) :1471-1476.
  • 9Manjit Singh, Mridul Garg. Durability of Cementing Binders Based on Fly Ash and Other Wastes[J ]. Construction and Building Materials, 2007, (21) :2012-2016.
  • 10Singh N B. Middendorf Calcium Sulphate Hemihydrate Hydration Leading to Gypsum Crystallization[J]. Progress in Crystal Growth and Characterization of Materials, 2007,53 ( 1 ) : 57-77.

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部