摘要
景德镇瓷坯料通常是以两种或两种以上的瓷石与高岭土所组成。本文研究了以星子高岭土,大洲高岭土,南港瓷石和三宝蓬瓷石所组成的景德镇瓷坯料系统。分别测定了在1050 、1180 、1260 和1310 ℃下烧成坯体的收缩率、吸水率、体积密度及显气孔率。
The body of Jingdezhen's porcelain are usually composed of two or more kinds of kaolin and china stone.The bodies of the Jingdezhen's porcelain are studied in this paper,that are composed of Xingzi kaolin,Dazhou kaolin,Nangang china stone and Sanbaopeng china stone.That are determined whose shrinkage,the water absorption,the bulk density and the apparent porosity of all bodies,that bodies are fired separately at 1050℃,1180℃,1260℃and 1310℃.It is discussed in the paper that relations between those properties at different firing temperature and the composition of those bodies.
出处
《陶瓷学报》
CAS
1999年第2期92-98,共7页
Journal of Ceramics
关键词
景德镇瓷
坯料组成
烧成温度
坯体
性能
Jingdezhen's porcelain,body composition,firing temperature,body property