摘要 采用电磁搅拌和熔体混合技术制备Al-20Si合金,研究表明,单纯采用电磁搅拌技术制备Al-20Si时,会产生偏析层,其初生Si相平均尺寸在60μm以上;而采用熔体混合+电磁搅拌复合处理可使Al-20Si合金中的初生Si相尺寸降至16μm以下,并消除在单纯电磁搅拌合金边缘出现的粗大的初生Si相的偏析层。熔体混合处理处理还可以强化过共晶Al-20Si合金的电磁搅拌效果,获得良好细化效果。 Al-20Si alloy was prepared by electromagnetic stirring and by melt-blending combining with electromagnetic stirring,respectively.The results indicate that a segregation layer can be observed in the Al-Si alloy prepared by electromagnetic stirring,in which the size of primary Si phase is more than 60μm,while coarse primary Si segregation occurred in edge of electromagnetic stirred Al-20Si alloy can be eliminated and size of primary Si phase can be refined to less than 16μm after combination treatment of melt-blending with electromagnetic stirring,which is attributed to melt-blending promoting the electromagnetic stirring effects on Al-20Si alloy.
出处 《特种铸造及有色合金》 CAS CSCD 北大核心 2010年第11期991-994,共4页 Special Casting & Nonferrous Alloys
基金 福建省教育厅资助项目(JA09173) 福建省科技计划项目(2010H002) 福州大学科技发展基金资助项目(600117)
关键词 Al—20Si合金 初生SI 熔体混合 电磁搅拌 细化 Hypereutectic Al-20Si Alloy,Primary Si Phase,Melt-blending,Electromagnetic Stirring,Refinement
  • 相关文献

参考文献11

二级参考文献138

共引文献265

同被引文献26

引证文献2

二级引证文献4

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部