对樟子松热处理材进行室内防霉、防蚁蛀及野外埋地检测,综合评价其耐久性能。结果表明:樟子松热处理材对霉菌、变色菌均无防治效力,不抗白蚁蛀蚀;樟子松热处理材的耐久年限约为3年。
Heat-treated Pinus sylvestris resistance against mould,fungi stain and termite attack was tested in our laboratory and the durability towards rot-fungi and termites was evaluated with our field test.The results showed that the heat-treated Pinus sylvestris did not resist mildew,termites,and blue-stain fungus.The two-and-half year field tests in Guangzhou showed the control samples decay resistance to be at the zero classification while the heat-treated wood was at the 9.5 classification.However,the classification rating for termite resistance was only two for the heat-treated samples.
出处
《木材工业》
北大核心
2011年第1期44-46,共3页
China Wood Industry
基金
中国林科院林业新技术所基本科研业务费专项基金(CAFINT2008C10)
关键词
樟子松
耐久性
耐腐
防霉
防白蚁蛀蚀
Pinus sylvestris
durability
decay inhibition
mold inhibition
termite resistance