摘要
为了缓解煤矿钻井废弃泥浆排放处理难的问题,研究利用废弃泥浆配制成地面预注浆浆液,通过对研制的泥浆采用降黏改性处理后,浆液的密度及黏度降低;塑性强度缓慢增长,约15 h可以达到50 kPa。淮北矿业集团袁店二矿主井井筒的S孔注浆工程利用钻井泥浆注浆材料7 606m3,经井筒掘进测量,注浆段井筒剩余涌水量仅为3 m3/h,注浆效果达到优良。
In order to release the problems of the abandoned drilling mud discharging and treatment,the paper had a study on the preparation of the surface pre-grouting grout with the abandoned drilling mud.With the sticky reduction and modification treatment of the prepared mud,the density and sticky of the grout would be reduced.The plasticity strength of the grout would be slowly increased and could be reached to 50 kPa after about 15 h.The grouting project with S boreholes for the mine main shaft of Yuandian No.2 Mine,Huaibei Coal Mining Group had consumed the drilling mud grout of 7 606 m3.After the mine shaft excavation and measurement,the residual water inrush quantity at the grouting section of the mine shaft was about 3 m3/h and the grouting effect was excellent.
出处
《煤炭科学技术》
CAS
北大核心
2011年第1期37-39,43,共4页
Coal Science and Technology
基金
"十一五"国家科技支撑计划资助项目(2008BAB33B02)
关键词
废弃泥浆
注浆利用
黏土浆
地面预注浆
abandoned drilling mud
grouting application
clay grout
surface pre-grouting