摘要
纤维素酶处理纤维素纤维后再进行免烫整理,当酶处理时间为20min时,织物经、纬向断裂强度呈最大;当酶处理时间为8min时,织物经、纬向撕裂强力最大;当酶处理50min时,耐磨性最高;当酶处理30min时,织物免烫水洗平整度最好。
Easy-care finish of cellulose fibre treated by cellulose is carried out . If the time of cellulose treatment is 20 minutes, breaking tenacity both of warp and weft are maximum; if the time is 8 minutes, tearing strength are maximum; if the time is 50 minutes, wearability is the best; if the time is 30 minutes, wash-wear and smoothness is the best.