摘要
研究了3C(W )、16Mn、921 三种钢在南海榆林海域全浸、潮差、飞溅环境中暴露8 年的腐蚀行为。其中,921 钢在飞溅区具有优良的耐蚀性,而在全浸和潮差区耐蚀性不如3C(W)钢和16Mn 钢的。发现921 钢在全浸区暴露2 年后发生腐蚀率随时间增加而增大的“逆转”现象。
The corrosion behaviors of 3C(W), 16Mn and 921 steels are studied in the all submerged area, tide area and splash area in the Nanhai Sea Yulin water for 8 years. It is revealed that in the splash area the corrosion resistance of 921 steel is more excellent than that of 3C(W) and 16Mn steels, while worse in the all submerged area and splash area. In the all submerged area, the corrosion rate of 921 steel decreases in the first two years and then increases with the time going on.