摘要
采用普通细度磷渣粉配制出了符合设计要求的C50T梁混凝土,其合宜掺量为20%。与矿渣粉和I级粉煤灰相比,普通细度磷渣粉配制的C50T梁混凝土的力学性能、抗渗性能显示出一定的优势,早期水化热和水化放热速率降低效果最明显。
The C50 T-beam concrete was prepared from the general fineness phosphorus slag powder in the article,and the appreciate dosage ofthe phosphorus slag powder is 20%.Compared with the Fly ash concrete and the Slag concrete,it shows a few advantage in its mechanical and impermeability property,especially it can decrease the total hydration heat and lower the exothermic process obviously at the earlier stage of hydration.
出处
《混凝土》
CAS
CSCD
北大核心
2011年第2期128-130,133,共4页
Concrete
关键词
普通细度磷渣粉
T梁混凝土
配制
性能
generally fineness phosphorus slag powder
T-beam concrete
preparation
property