高产碳沥青的制备和性能研究 被引量:9

PREPARATION AND PROPERTY OF HIGH CARBON YIELD PITCH
下载PDF
导出
摘要 研究了硫化沥青的组成和结构与其产碳率、流变性能和热稳定性能的关系. 结果表明, 硫化法调制煤沥青在软化点170℃~200℃范围内, 产碳率高, 热稳定性好, 是较理想的浸渍剂. By researching the reaction properties, relation between the consist, structure of sulfuretted pitch and its carbon yield,rheologic property at high temperature, thermal stability, a method of preparing high carbon yield pitch and its impregnating properties were studied. The results showed that the pitch prepared by sulphuration, when its softening point is in the range of 170℃ to 200℃, have high carbon yield (>65%), and good rheologic property and good thermal stability.\;
出处 《煤炭转化》 CAS CSCD 1999年第4期79-83,共5页 Coal Conversion
关键词 高产碳 沥青 浸渍剂 硫化 制备 high carbon yield, pitch based impregnant, sulphuration
  • 相关文献

参考文献1

  • 1Liu Guangzheng,University Karlruhe Vorgelegte und Genehmigte,1989年

同被引文献100

  • 1李太平,王成扬.针状焦技术的研究进展[J].炭素,2004(3):11-16. 被引量:26
  • 2徐军装.环氧煤沥青特强级防腐[J].化工施工技术,1996,18(5):45-46. 被引量:1
  • 3常宏宏,魏文珑,王志忠,杨怀旺,姚润生.煤沥青的性质及应用[J].山西焦煤科技,2007(2):39-42. 被引量:22
  • 4何丙林 苏振立.工业二乙烯基苯的分离[J].离子交换与吸附,1988,4(2):81-83.
  • 5许斌,付苏平,虞继舜,陈鹏.净化煤沥青的制备及其性质表征[J].炭素,1997(2):15-18. 被引量:14
  • 6Li X K,Li O T. Rheological properties and carbonization of coal-tar pitch. Fuel, 1996,75 (1): 3.
  • 7Matzinos P D, Patrick J W, Walker A. Coal-tar pithc as a matrix precursor for 2-D C/C composites. Carbon, 1996,34.(5):639.
  • 8Matzinos P D,Patrick J W ,Walker A. The void structure of 2-D C/C preforms and composites: Effect of the nature of the matrix precursor coal-tar pitch. Carbon, 1997,35 (4) :507.
  • 9Blanco C, Santamaria R, Bermejo J, et al. Separation and characterization of the isotropic phase and coexisting mesophase in thermal treated coal-tar pitches. Carbon,2000,38(8) :1169.
  • 10Guillen M D,Dominguez A,Iglesias M J,et al. Analysis of coal tar pitch: Relations between thermal behaviour and composition. Fuel, 1996,75 (9) : 1101.

引证文献9

二级引证文献52

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部