Research on Voids Deformation Welding Condition for Manufacturing of Heavy Forgings 被引量:1

Research on Voids Deformation Welding Condition for Manufacturing of Heavy Forgings
原文传递
导出
摘要 Crushing and diffusion welding are two critical healing stages of interior void defects in heavy forgings.The healing result depends on many factors during the forging process,such as stress,temperature,deformation and type of material,while the void diffusion welding condition is still not well known at the present.This paper is concerned with the deformation welding condition of the closed void interface in heavy ingot during the hot forging process.A void crushing experiment is carried out to recognize the microstructure of the closed void interface.According to the healing mechanism at high temperature,a new physical simulation model is setup to study the deformation welding process of the closed void interface based on the theory of atom diffusion and the interface contact mechanics prototype.Compared with the experimental results,the influence of deformation degree,forming temperature and holding time on the welding quality is discussed,and then the deformation welding condition of closed void interface is presented.The proposed condition helps to improve forging technology and product quality. Crushing and diffusion welding are two critical healing stages of interior void defects in heavy forgings. The healing result depends on many factors during the forging process, such as stress, temperature, deformation and type of material, while the void diffusion welding condition is still not well known at the present. This paper is concerned with the deformation welding condition of the closed void interface in heavy ingot during the hot forging process. A void crushing experiment is carried out to recognize the microstructure of the closed void interface. According to the healing mechanism at high temperature, a new physical simulation model is setup to study the deformation welding process of the closed void interface based on the theory of atom diffusion and the interface contact mechanics prototype. Compared with the experimental results, the influence of deformation degree, forming temperature and holding time on the welding quality is discussed, and then the deformation welding condition of closed void interface is presented. The proposed condition helps to improve forging technology and product quality.
出处 《Journal of Shanghai Jiaotong university(Science)》 EI 2011年第2期203-208,共6页 上海交通大学学报(英文版)
基金 the National Natural Science Foundation of China (Nos.50435010 and 51005197) the National Scientific and Technical Supporting Programs of China (No.2007BAF02B12) the Doctor Fund Project of Yanshan University (No.B298)
关键词 large forgings interior void defects physical simulation deformation welding condition large forgings, interior void defects, physical simulation, deformation welding condition
  • 相关文献

参考文献11

  • 1Jin Ning. Investigation of collapse and welding law of cavities and porous defects in large forgings, and development of high temperature moir6 grids [DJ. Beijing: Department of Mechanical Engineering, Tsinghua Uni- versity, 1996 (in Chinese3.
  • 2BI Qing-xia. Study on hole seaming of large forgings by diffusing under high temperature [D]. Qinhuangdao: Institute of Mechanical Engineering,Yanshan University, 2004 (in Chinese).
  • 3黄华贵,杜凤山,许志强.影响大锻件内部孔隙性缺陷扩散焊合的因素[J].钢铁研究学报,2007,19(11):55-59. 被引量:9
  • 4PARK C Y, YANG D "Y'. A study of void crushing in large forgings. I, Bonding mechanism and estimation model for bonding efficiency [J]. Journal of Material Processing Technology, 1996, 57(1-2): 129-140.
  • 5PARK C Y, YANG D Y. A study of void crushing in large forgings. Ii. Estimation of bonding efficiency by finite-element analysis [J]. Journal of Material Processing Technology, 1997, 72(1): 32-41.
  • 6PARK C Y, YANG D Y. Modelling of void crushing for large-ingot hot forging [J]. Journal of Materials Processing Technology, 1997, 67(1-3): 195-200.
  • 7钟约先,袁朝龙,马庆贤.材料内部裂纹自修复中组织生长机制[J].清华大学学报(自然科学版),2002,42(4):512-515. 被引量:10
  • 8MA Qing-xian, WANe Zhi-cheng, ZHONG Yue-xian. The mechanism of faults originating from inclusions in the plastic deformation processes of heavy forging [J]. Journal of Material Processing Technology, 2002, 123(1]: 61-66.
  • 9YUAN Chao-long, ZHONG Yue-xian, MA Qing-xian. Mimic biology research on self-recovering mechanism of cavity type crack [J]. Science in China Series E, 2002, 45(5): 531-540 (in Chinese).
  • 10MARSION L W, PRICE S, ]V[EES J, et al. Improved in-service performance of large forged back up rolls through the development of steel chemistry [C]. Proceedings of Rolls 2000+ Advances in Mill Roll Technology. Birmingham, UK: IOM Communications Ltd, 1999: 281-291.

二级参考文献20

共引文献52

同被引文献15

  • 1狄国标,刘振宇,郝利强,刘相华.海洋平台用钢的生产现状及发展趋势[J].机械工程材料,2008,32(8):1-3. 被引量:68
  • 2蔡得祥,李金富.大型特厚板用扁钢锭的研制[J].宝钢技术,2007(4):45-48. 被引量:14
  • 3刘鹏,刘坤,冯亮花.定向凝固技术的发展及在特厚钢板生产中的应用[J].鞍山科技大学学报,2007,30(5):473-477. 被引量:8
  • 4Jun Hu,Lin-Xiu Du,Hui Xie,Xiu-Hua Gao,R.D.K. Misra.Microstructure and mechanical properties of TMCP heavy plate microalloyed steel[J]. Materials Science & Engineering A . 2014
  • 5T.L. Fu,Z.D. Wang,Y. Li,J.D. Li,G.D. Wang.??The influential factor studies on the cooling rate of roller quenching for Ultra Heavy Plate(J)Applied Thermal Engineering . 2014
  • 6Hong-bo Xia,Shao-gang Wang,Hai-feng Ben.??Microstructure and mechanical properties of Ti/Al explosive cladding(J)Materials and Design . 2014
  • 7Yu-an Jing,Yi Qin,Xiaoming Zang,Yinghong Li.??The bonding properties and interfacial morphologies of clad plate prepared by multiple passes hot rolling in a protective atmosphere(J)Journal of Materials Processing Tech. . 2014
  • 8S.A. Hosseini,M. Hosseini,H. Danesh Manesh.??Bond strength evaluation of roll bonded bi-layer copper alloy strips in different rolling conditions(J)Materials and Design . 2010 (1)
  • 9H. Danesh Manesh,A. Karimi Taheri.??Theoretical and experimental investigation of cold rolling of tri-layer strip(J)Journal of Materials Processing Tech. . 2004 (2)
  • 10钱振伦.宽厚板坯连铸技术和宽厚板生产[J].中国钢铁业,2010(7):30-32. 被引量:4

引证文献1

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部