摘要
以部分白灰代替白云石,提高炉渣三元碱度,提高炉温,可使[S]下降,合金质量基本稳定,炉况良好。
Lime was used part istead of dolomite to icrease terary basicity of slag ad to elevate furace temperatute for decreasig [S].This resulted i steady metal quality ad well operatioal performace.
出处
《铁合金》
北大核心
1990年第3期9-10,共2页
Ferro-alloys