摘要
介绍GL-2 型直径600m m 螺旋选矿机在攀枝花10 万t选钛厂粗选段选别粗粒级(0.4~0.1m m )的工业试验和生产应用,结果表明,该机同原生产上使用的铸铁直径600m m 螺旋选矿机相比,选别指标好,提高作业回收率13% ,适应性强,使用寿命长,节省了生产费用。
The industrial test and production application of D600mm Type GL\|2 spiral concentrator in Panzhihua titanium mineral processing plant for beneficiating the coarse grain particles (0\^4~0\^1mm) at the roughing stage are described. Results indicate that compared with the originally\|used cast iron spiral concentrator with the diameter of 600mm, this new concentrator is characterized by good beneficiation results, strong adaptability and long lifetime; the operational recovery can be increased by 13%; the production cost is saved and the technical and economic indexes of the Ti mineral processing mill are improved.
出处
《广东有色金属学报》
1999年第2期106-110,共5页
Journal of Guangdong Non-Ferrous Metals