摘要
溶胶-凝胶法制备单相性、均匀性较好的La(1-x)SrxMnO3(x=0.1,0.2,0.3,0.4,0.5)纳米微粉系列样品,并用X射线衍射分析样品的结构类型.考察样品的烧结特性和高温电导率随晶粒尺寸的变化规律.通过电池伏安特性曲线的测量,对锰酸锶镧作为(ZrO2)0.92(Y2O3)0.08电解质燃料电池阴极的性能进行研究.
In this paper, the La1-xSrxMnO3 (x = 0. 0 ~ 0. 5 ) nanoparticles were prepared by sol-gel method. The phase composition and structure of the saTnples were analysed by Tneans of X-ray diffraction. Electrlcal properties of the samples wele detected. I-V characterlstics of as the cathode of the (H2/H2O ) -Ag/ (Zro3 ) 0. 02 (Y2O3 ) 0.08/ La1-xSrxMnO3,-air fuel cell were tested.
出处
《吉林大学自然科学学报》
CAS
CSCD
1999年第4期44-46,共3页
Acta Scientiarum Naturalium Universitatis Jilinensis
基金
国家计划委员会"八五"重点攻关项目!715-21-02
国家教委博士点基金!9118309
关键词
燃料电池
阴极
高温电导率
制备
阴极材料
SOFC,cathode,La_(1-x)Sr_xMnO_3,high-temperature electrical conductivity