摘要
本文根据我厂大件扁平产品( 口径在203 m m 以上) 釉面光泽度差的问题进行了全面分析、研究,成功研制出在1250 ~1330 ℃烧成的高光泽日用瓷釉配方,解决了大件扁平产品釉面光泽度差的问题,并探讨了主要原料在釉料中的作用及用量范围。
The Problem of the poor gloss of the glaze for the large flatware(outside diameter above 203mm)was completely analysed and studied.Based on successful development of the batch composition for high gloss glaze for the chinaware at the problem of the poor gloss for the glaze for the large flatware was solved and the action and the dosage of major raw materials in the glaze were researched.
出处
《山东陶瓷》
CAS
1999年第3期28-31,40,共5页
Shandong Ceramics