摘要 在试验研究基础上,提出了一种提高含砷金精矿二段焙烧—氰化浸出工艺金浸出率方法。试验结果表明,含砷金精矿经一段焙烧(450~500℃)除砷后,加入一定量的添加剂SR,再进行二段焙烧(630~650℃),然后经稀硫酸除铜后进行氰化浸出,可使金的氰化浸出率提高4.65%。该方法可获得较好的经济效益和社会效益。 Based on experimental researches,a two-stage roasting and cyanidation technique is proposed to enhance the gold leaching rate of a gold concentrate containing arsenic.After the first stage roasting(450~500 ℃) to remove arsenic,an additive SR is added before the second stage roasting(630~650 ℃),and then dilute sulphuric acid is used for copper removal,the final process is cyanidation leaching.The test results show that the leaching rate of gold increases 4.65%,and good economic and social benefits are obtained.
出处 《黄金》 CAS 北大核心 2011年第6期48-49,共2页 Gold
关键词 含砷金精矿 二段焙烧 氰化 浸出率 gold concentrate containing arsenic two-stage roasting cyanidation gold leaching rate
  • 相关文献

同被引文献75

引证文献10

二级引证文献59

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部