主要通过气泡点的检测和硫化程度的计算等方法优化了轮胎硫化时间。硫化测温及减时耐久性测试结果表明,9.00R2016PRS811型轮胎存在一定程度的过硫,轮胎性能未达到最佳状态。在保证轮胎性能的前提下,将硫化时间由原来的54m in缩短至48m in,减少了能耗,提高了生产效益。
The curing time for the tire 9.00R2016PRS811 was optimized by mainly using the methods of the test of blowing points and the calculation of cure degree.The results of the curing temperature-measuring and the durability experiments of cured tire showed that the tire 9.00R2016PRS811 was overcured to a certain extent,and the properties of cured tire did not attain to the optimum.The cure time of the tire 9.00R2016PRS811 was shortened from 54 min to 48 min as ensuring the properties of cured tire,and the energy consumption was reduced,and the productivity was increased.