摘要
试验依据高硫复杂铜铅锌矿矿石性质的特点,采用磁选—浮选联合工艺流程。试验工艺流程关键技术是磁选脱除磁黄铁矿,应用优先浮选流程,优先浮选铜精矿进行铜硫分离,铜与铅锌分离采用高效抑制剂组合无氰无铬清洁分离工艺,获得了良好的试验指标,铜精矿、铅精矿、锌精矿的品位分别为21.96%、50.68%、41.58%,回收率分别为68.13%、52.24%、79.77%,为高硫复杂难选铜铅锌选矿提供了新途径。
According to the high-sulphur complex copper-lead-zinc mine ore properties,magnetic separation-floatation flow united technical process flow was used in this test.The key technology of the process is removing pyrrhotite by magnetic separation and using selective flotation process to separate copper and sulphur.Dissolvable depressants compound free of cyanide and chromium was used to separate copper and lead.Excellent test index were gained with the grade of copper concentrate,lead concentrate and zinc concentrate was 21.96 %,50.68 % and 41.58 % and the recovery rate was 68.13 %,52.24 % and 79.77 % respectively,this work provide a new way for the high-sulfur complex copper-lead-zinc mine.
出处
《有色金属(选矿部分)》
CAS
2011年第1期1-5,共5页
Nonferrous Metals(Mineral Processing Section)
关键词
高硫复杂铜铅锌矿
磁选—浮选联合工艺流程
优先浮选
环保型抑制剂组合
high-sulfur complex copper-lead-zinc mine
magnetic separetion-floatation united technical flow
selective flotation
dissolvable depressants compound