摘要 研究了喷射成形Al93 .5Cu3Fe1 .5 Ni1Ce0 .5Zr0 .5 合金快速凝固组织特征及弥散强化相的形成。结果表明, 喷射成形快速凝固技术显著地细化了合金组织; 预成形毛坯具有3 种典型的组织特征, 其中主要弥散强化相为具有立方晶体结构、晶格常数a = 0 .852 nm 的Al17Cu4FeNiCe The characteristic microstructures and formation of dispersoid of spray formed Al 93.5 Cu 3Fe 1.5 Ni 1Ce 0.5 Zr 0.5 alloy were investigated. The observation results showed that the microstructures of deposit are fine and homogeneous and there exist three kinds of typical formation mechanisms of microstructures in deposit. The main dispersoid in deposit is Al 17 Cu 4FeNiCe phase with complicated cubic crystal structure whose lattice constant keeps 0.852 nm.
出处 《中国有色金属学报》 EI CAS CSCD 北大核心 1999年第A01期125-130,共6页 The Chinese Journal of Nonferrous Metals
关键词 快速凝固 喷射成形 铝合金 微观组织 rapid solidification spray forming high strengthened aluminium alloy microstructure
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部