摘要
分析了济钢三炼钢厂1#连铸机中间包连浇炉数偏低的原因,通过改进中间包预热与烘烤制度、连铸功能耐材、低过热度浇注等,提高了中间包的连浇炉数,达到了降低成本、提高连铸机作业率的目的。
It is analyzed the reason for casting heats of tundish of No.1 caster of No.3 Steelworks of Ji Steel being little low.The casting heats are increased with improvement of pre-heating and toasting system,continuous casting function refractory materials,low-superheating casting.